B1 | B2 | B4 | B5 | B6 | B7 | ||
JIS Classification | 900-0.70-0.26 | 1000-0.70-0.28 | 1200-0.80-0.37 | 1300-0.80-0.39 | 1400-0.90-0.42 | 1500-1.00-0.50 | |
Specification | Permanent Linear Change Not more than ±2% when tested at(℃) | 900 | 1000 | 1200 | 1300 | 1400 | 1500 |
Bulk Density | 0.70≧ | 0.70≧ | 0.80≧ | 0.80≧ | 0.90≧ | 1.00≧ | |
Thermal Conductivity at 600℃ [W/m・K] |
0.26≧ | 0.28≧ | 0.37≧ | 0.39≧ | 0.42≧ | 0.50≧ | |
Test Result | Bulk Density | 0.65 | 0.65 | 0.78 | 0.78 | 0.86 | 0.75 |
Cold Crushing Strength [MPa] |
3 | 3.2 | 1.5 | 1.7 | 2.4 | 4 | |
Thermal Conductivity at 600℃ [W/m・K] | 0.22 | 0.26 | 0.33 | 0.33 | 0.37 | 0.41 | |
Permanent Linear Change % at ( )℃X12hr | -0.6 | -0.8 | -0.3 | -0.25 | -1 | -0.9 | |
-900 | -1000 | -1200 | -1300 | -1400 | -1500 |